COLOUR. PROTECTION. POSSIBILITY.

EXPERT ADVICE · 0800 222 423

DEKRO How-To

Specifications for
surface coatings.

From plaster and timber to metal and specialist applications: select a surface to read the preparation guidance and coating system.

Showing 24 of 24 entries

No matching entries. Try another search or clear the filters.

Cement Plaster Masonry & board

General:

With new cement plaster problems arise mainly from three factors:

  1. The presence of moisture.
  2. The alkaline nature of some of the surfaces, and the presence of soluble crystalline salts.
  3. Water is used in large quantities in new structures and until such time as walls, ceilings, pillars, soffits, etc. have dried out, it is dangerous to apply paints which seal the surface and prevent the natural evaporation of the water still deep in the plaster. An impermeable paint will entrap the moisture which will cause blistering and flaking.

Brickwork, concrete and cement plaster are alkaline from the cement and whilst some of the proprietory skim plasters are not intrinsically alkaline, they can become alkaline if the plasterer adds unslaked lime for easier working. Alkaline salts can leach from brick or cement backings during the drying out process. In the presence of moisture, the alkaline salts will attack the binder in oil paints, causing softening (saponification) of the paint.

The surest way of avoiding problems on these surfaces is to postpone painting until drying of cement plaster is complete, but unfortunately this is rarely possible as plaster can sometimes take many months to dry. When decoration must be carried out at an early stage, the paints used should interfere as little as possible with the drying process and be alkali resistant. In such cases “oil” paints cannot be used as they seal the surface and are attacked by free alkali. Fortunately the modern masonry and acrylic emulsion paints allow free passage of moisture in the wall without affecting the paint film. Of great importance is that this is a one-way passage, ie., water vapour can escape through the acrylic or masonry paint film from the wall to the atmosphere but water cannot penetrate the paint film back into the wall.

Another problem for which there is no cure, not even in the case of 100% acrylic paints, is efflorescence, or the development on the surface of a white crystalline deposit, which is due to the crystallisation of soluble salts formed during drying out, and their growth beneath a paint film will force off the coating. Efflorescence often occurs in the following areas: (i) ground level below dampcourse, (ii) lower portion of walls where there is no dampcourse, (iii) below leaking windowsills, (iv) near ceilings from roof leaks and (v) from leaking pipes in walls.

Preparation:

New plaster is not normally subject to cracking initially. Remove dust, dirt, plaster splashes. Clean down generally.

Previously limewashed or distempered:
Remove to bare plaster by wire brushing, scraping or high-pressure water blast. Cut out cracks and imperfections, fill and sand smooth when dry.

Previously oil, enamel, P.V.A. or acrylic painted:
If the existing paint is in poor condition, remove by scraping or with Dekro Super Paint Stripper. Wash down with a suitable concentrated detergent, rinse and allow to dry. Cut out cracks and imperfections, fill with a recommended crack filler and sand smooth when dry.

If the existing paint is in good condition, wash with a sugar soap solution and rinse clean, or with a suitable solvent to remove dirt, grease, wax polish or other contaminants. Sand glossy surfaces with a suitable abrasive. Rinse clean and allow to dry.

Painting:
N.B.: Allow minimum of overnight drying time for an oil and alkyd-based paint to allow for seasonal low temperatures.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Skimmed Plaster Masonry & board

General:

See general comments under “Cement Plaster”. Another factor to be taken into account in the case of skimmed plaster, in addition to age, is its texture. With patent plasters such as Glass-stone, Cretestone, other gypsum or keenes types, the surfaces are sometimes trowelled so smooth, compact and hard as to be an almost marble-like finish. Special care must be exercised in the choice of the correct primer coat, as there is often a layer of fine powder on these surfaces. Skimmed plasters are only used on interior walls.

Preparation:

New:
Remove dust, dirt, plaster splashes. Cut out cracks and imperfections, fill and sand smooth when dry.

Previously limewashed or distempered:
Remove to bare plaster. Cut out cracks and imperfections, fill and sand smooth when dry.

Previously oil, alkyd, P.V.A. or acrylic painted:
If the existing paint is in poor condition, remove by scraping or with Dekro Super Paint Stripper. Wash down with a suitable concentrated detergent, rinse and allow to dry. Cut out cracks and imperfections, fill and sand smooth when dry.

If the existing paint is in good condition, wash with sugar soap and water, a suitable concentrated detergent or suitable solvent to remove dirt, grease, wax polish or other contaminants. Abrade glossy surfaces to form a key for subsequent coats. Rinse and allow to dry.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Fibre/Asbestos Cement Masonry & board

Asbestos-containing or suspected materials

Do not scrape, sand, dry-brush or pressure-clean material that may contain asbestos. Stop and seek advice from a suitably qualified asbestos specialist before any preparation or coating work. Read NIOH asbestos guidance.

General:

Fibre/Asbestos cement occurs in several forms in buildings, mainly as wall partitions, ceilings, roofing sheets (plain, corrugated), tiles, gutters and down pipes. This material is very absorbent, often highly alkaline, and may contain relatively high concentrations of salts.

“Oil” paints may not be used on new exterior fibre cement surfaces. Blistering and peeling may be caused by moisture which may persist due to entry from the back of the surface, e.g. when gutter, downpipes, etc., are not internally painted and the continued flow of rainwater maintains damp conditions within the asbestos cement.

Fibre/Asbestos cement should be dry before painting. Gutters, (bituminous solution is recommended for inside of gutters), window sills, fascia boards, etc., should be painted on both sides to prevent moisture penetration. For external asbestos cement surfaces, 100% acrylic type emulsion paints or Dekrolite Masonry Paint are preferred because of their high alkali resistance.

Fungus tends to grow on unpainted asbestos cement because it is alkaline and porous, holding moisture and food for spores. It is therefore highly recommended to waterproof unpainted surfaces with Aquablock Water Repellent.

Preparation and coating

Preparation and coating of asbestos-containing surfaces require specialist assessment. Contact DEKRO technical support and a suitably qualified asbestos specialist for a project-specific system.

Bricks Masonry & board

General:

Brickwork presents a particularly variable surface for painting and often paint failures may be isolated to individual bricks owing to great differences in porosity, or to the presence of salts causing efflorescence with its attendant flaking, or the presence of coloured substances such as iron salts causing severe staining especially of water-based paints. Certain types of bricks have highly glazed surfaces and offer a poor key for paint systems. In addition, the greasy film of firmly adherent dirt and grime may cause subsequent flaking. Old exposed brickwork may have a loose powdery surface.

Preparation:

New:
Remove dust, dirt, plaster splashes.

Previously limewashed or distempered:
Remove to bare surface by wire brushing, scraping or washing.

Previously oil, alkyd, P.V.A. or acrylic painted:
If in poor condition remove to original surface; if in good condition clean to remove dirt, grease, etc.

Painting

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Brick Dressing

First Coat: Hydroglaze/Aquablock
Second Coat: Hydroglaze/Aquablock

Tiles Masonry & board

General:

Apart from glazed tiles which are available in a wide range of colours and do not normally require painting, a cheaper cement tile is used by the building industry on roofs, windowsills, etc. N.B.: This specification does not refer to floor and wall tiles.

Preparation:

New:
Remove dust, dirt, plaster splashes.

Previously oil, alkyd, P.V.A. or acrylic painted:
If in poor condition remove to original surface; if in good condition clean to remove dirt, grease, etc.

Unpainted covered with fungus:
Remove visible fungi and dirt. Apply one coat Hydrowash Fungicidal. Allow to dry then brush down with stiff bristle brush.

Rinse with clean water and allow to dry.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Wood Painted Timber

General:

When wood is moisture-laden or unseasoned, the applied paint film will inevitably break down through blistering, cracking, flaking or peeling. When timber arrives on the site in a satisfactory condition, it is often inadequately protected from the weather and rapidly absorbs moisture. It is therefore essential that dry, unprimed timber arriving on site is properly prepared and primed at the earliest opportunity.

All faces and edges must be primed, especially surfaces which will be inaccessible after fixing and will absorb moisture from adjacent brickwork or plaster if unprotected. Special attention should be given to end grain where two coats of primer are recommended.

Wood primers are best applied by brush to ensure that the paint is forced well into the pores of the wood. Joinery stacked on site, even when primed, must be covered to protect it from the weather as a single coat of primer cannot give adequate protection. The use of poor quality primers is false economy and likely to cause breakdown of the whole paint system.

On previously painted surfaces where flaking has occurred, the bare wood may have been exposed to the weather for many months. Unless these surfaces are allowed to dry, there is little chance of the repainting being successful.

Wood which has been exposed for a lengthy period without paint, often becomes denatured and fibirous and in this condition it affords a poor key for paint. In such cases the perished outer layer must be removed by scraping and sanding before applying the primer.

Preparation:

New:
Remove dust, dirt, grease, etc. Sandpaper smooth and dust off.

Previously oil, alkyd, P.V.A. or acrylic painted:
If the existing paint is in poor condition, remove by scraping, burning or with Dekro Super Paint Stripper. Wipe down with a suitable solvent, sand smooth and dust off. If the existing paint is in good condition, wash down with a sugar soap solution, a suitable detergent solution or solvent to remove dirt, grease, wax polish or other contaminants. Sand down glossy surfaces with a suitable abrasive. Rinse and allow to dry thoroughly.

Dekro Zinc Phosphate Primer to nailheads. Stop and fill nailheads with Plastic Wood and sand smooth.

First Coat: Dekro Pink Wood Primer
Second Coat: Dekro Universal Undercoat
Third Coat: Suitable Top Coat
Fourth Coat: Suitable Top Coat

Dekro Adthane Polyurethane Enamel

First coat: Dekro Adthane Enamel thinned 20%  with polyurethane thinners
Second coat: Dekro Adthane Enamel
Third coat: Dekro Adthane Enamel

Wood Varnished Timber

General:

The natural beauty of wood is enhanced by the application of clear varnish, which can be used on both soft and hard woods. However, no clear varnish system on wood will stand up for any length of time if the surface is fully exposed to weather. Ultraviolet rays from the sun penetrate the transparent varnish and destroy the structure of the wood causing loss of adhesion and subsequent flaking. Varnishes containing transparent pigments which are U.V. absorbers, are the only varnishes that should be used on exterior exposed natural timber.

Preparation:

New:
Clean to remove dirt, plaster splashes, etc., rub down smooth with sandpaper and dust off.

Previously stained, varnished or lacquered:
If in poor condition, remove all existing stain, varnish or lacquer with Dekro Super Paint Stripper or a strong washing soda solution (1kg per 5 litres warm water), and steel wool. Wash down with vinegar water (1 litre vinegar to 5 litres water) and bleach to a uniform colour with a 10% Oxalic Acid Solution. Neutralize with domestic ammonia, rinse with clean water and leave to dry. Sand smooth and dust off.

Note:

  1. Oxalic acid is highly toxic.
  2. Light woods such as maple and birch cannot be treated as above.
  3. After the above treatment the wood must be absolutely dry before coating.

If in good condition, wash down with sugar soap and water, or solvent to remove dirt, grease, wax polish, etc. Rub down smooth with sandpaper to a matt finish and dust off.

Previously waxed:
Wash down thoroughly with Dekro Wunda Clean or suitable concentrated detergent to remove all traces of Wax, rinse and allow to dry thoroughly. Rub down and dust off. Do a test patch to be sure all wax has been Removed before coating the whole area.

Dekro Timbertek (Interior/Exterior)

First coat: Dekro Timbertek thinned 20% with turps
Second coat: Dekro Timbertek
Third coat: Dekro Timbertek

N.B.: Sanding between coats.

Dekro Glossy Polyurethane Varnish (Interior)

First coat: Dekro Sanding Sealer. Omit over previously varnished surfaces in good condition
Second coat: Dekro Glossy Polyurethane Varnish
Third coat: Dekro Glossy Polyurethane Varnish

Dekro Eggshell Polyurethane Varnish (Interior)

First coat: Dekro Sanding Sealer. Omit over previously varnished surfaces in good condition
Second coat: Dekro Eggshell Polyurethane Varnish
Third coat: Dekro Eggshell Polyurethane Varnish

Dekro Matt Polyurethane Varnish (Interior)

First coat: Dekro Sanding Sealer. Omit over previously varnished surfaces in good condition
Second coat: Dekro Matt Polyurethane Varnish
Third coat: Dekro Matt Polyurethane Varnish

Dekro Spar Varnish (Interior/Exterior)

First coat: Dekro Sanding Sealer for interior work. Omit over previously varnished surfaces in good condition
Second coat: Dekro Spar Varnish
Third coat: Dekro Spar Varnish

Dekroguard (Exterior Wood Treatment)

First coat: Dekroguard thinned 20% with turps
Second coat: Dekroguard
Third coat: Dekroguard Clear

Note: Dekroguard should only be used over bare wood.

Composition Board Masonry & board

General:

Many types of composition boards, such as woodpulp (fibre) board, gypsum board, acoustic board, asbestos cement board, woodchip board, etc., are used in building constructions.

Fibre building boards tend to warp or buckle if used in humid conditions and under these circumstances it is advisable to paint the backs and edges before fixing. The fibres of some soft fibre boards may be raised if water paints are applied to them and where appearance is important, care must be taken that the paint does not fill the texture as this will impair the acoustic properties. Flat paint, using the minimum number of coats, gives the best results.

Although the harder grades of fibre boards (such as masonite) have a hard, polished surface, they should not be rubbed down, as abrasion will score the board and spoil its appearance. Some of these hardboards contain water soluble materials which bleed into and discolour waterpaints if not sealed off first with an “oil” paint.

Preparation:

New:
Dust off.

Previously distempered:
It is extremely difficult to remove existing powder distemper from composition boards completely without damaging the face of the board through excessive wetting and scraping. Therefore remove as much of the distemper by careful dry sanding and dust off loose powder.

Previously oil, alkyd, P.V.A. or acrylic painted:
If the existing paint is in poor condition, remove to bare surface by careful scraping and dry sanding, dust off powder. If in good condition, clean down to remove dirt, grease, etc. Sand glossy surface and dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Paper Masonry & board

General:

Whilst it is not usual to paint paper, it may on occasions be found desirable to do so, eg. overpainting of wallpaper, liningpaper, etc. “Oil-based” paints should not be applied to paper because they harden and embrittle progressively with age.

Wallpaper adhesive remains water soluble and the paper would automatically bubble due to expansion and softening of the adhesive when overcoated with water based paints. These bubbles usually disappear when the paint dries.

Preparation:

Dust off. Ensure that the paper is adhering firmly.

Dekro Hydroglaze (Interior/Exterior)

A coat of Dekro Hydroglaze confers washability to wallpaper.
Not recommended for wallpapers containing mica.

Painting

First Coat: Suitable Top Coat
Second Coat: Suitable Top Coat

Metal Ferrous Metals

General:

The protection of iron and steel is a serious problem, and many millions of rands are spent annually to prevent or limit corrosion and on replacement of corroded metal.

The important factors in the protection of iron and steel by painting are:

  1. The thoroughness of the preparatory work before painting.
  2. The type of primer used.
  3. The thickness of the paint system.

As far as preparatory work is concerned, it has been shown that the effective life of a paint coating of perfectly clean steel, free from rust and scales, may be up to five times longer than that of the same coating applied to imperfectly cleaned steel. The traditional manual methods of preparing new and old steelwork for painting by chipping, scraping and wirebrushing are far from ideal, as they cannot remove lightly-adherent scale nor deal effectively with rust on pitted or rough surfaces. Alternative methods such as pickling, grit blasting, flame cleaning and chemical derusting are either not practical on erected steel, or may be considered too expensive. It should be realised that the higher initial cost would be more than offset by a reduction in maintenance costs by the longer life of the paint coatings.

For general use on iron and steel, primers incorporating rust-inhibitive pigments must be used, for example, zinc phosphate, metallic zinc, etc., in various binders such as the conventional linseed oil, or alkyd resins, or epoxy resins, etc. Too often cheap and inferior primers are used containing less than the minimum quantities of anti-corrosive pigments to be effective. Such paints do more harm than good as they must first be removed before a systematic and effective painting operation can be carried out.

Steelwork must be primed as soon as possible after it has been prepared, whether on site or at the manufacturer’s works, as even a few hours exposure in a damp or contaminated atmosphere will nullify the value of thorough preparation. The thickness of the overall paint is important and at least three full coats must be applied.

Preparation:

New:
Clean down to remove dirt, grease, oil, etc. Sand or grit blast to remove all rust and millscale. If sandblasting is not economically viable, chip, scrape or wirebrush to remove rust and loose scale back to clean metal. Where it is not possible by manual methods to remove rust from pitted or rough surfaces, apply a proprietory rust convertor such as Dekro Hydromet (RCC) or a similar product in accordance with the manufacturer’s instruction. Cleaned and/or treated surfaces must be primed immediately.

Previously painted:
If in poor condition, remove by scraping, burning or with Dekro Super Paint Stripper. Then proceed as for new substrate. If in good condition, clean down thoroughly with a suitable solvent to remove dirt, grease, oil, etc. Sand glossy surfaces with suitable abrasive and dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Metal Galvanised Metals

General:

A galvanised surface, especially when new, is particularly difficult to paint for the following reasons:

  1. It is so smooth and does not provide a good key for most paints.
  2. It is usually heavily pretreated by the steel manufacturer to prevent white rust on storage and this pre-treatment must be thoroughly removed before paint is applied.

Zinc as a metal can react with the ingredients in some paint to form salts between the paint and the surface, thus further reducing adhesion. It was the practice in years gone by, either to allow the galvanised iron to weather to obtain a surface receptive for paint, or to use mordants such as copper sulphate, vinegar, spirits of salts, etc. These methods are now obsolete having been proved technically unsound.

Preparation:

New:
Hose or rinse down with clean water to remove heavy dust, grit or organic matter. Clean down with Dekro Galv-O-Clean Degreaser or Galv-Etch by working over the surface using a mop, brush or hessian. Thoroughly rinse down with clean water to remove residues. Note whether the final rinsing water forms a continuous film over the surface. If it does, then cleaning is sufficient, if not, repeat the cleaning operation.

Previously painted:
If the existing paint is in poor condition, remove by scraping, burning or with Dekro Super Paint Stripper. Then proceed as for new work.

If the existing paint is in good condition wash down to remove dirt, grease, dust or other contaminants with a suitable concentrated detergent. Abrade glossy surfaces with a suitable abrasive and dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Metal Non-Ferrous Metals

General:

Aluminium and its alloys are widely used in building construction in the form of flat or ribbed sheets, extruded sections, cast components, etc. Whilst aluminium as a metal is largely self-protective because of its oxide layers, it may require paint for decoration or for protection under very severe corrosive conditions. Sheets and extruded sections have a smooth shiny surface and require pre-treatment to obtain a satisfactory key for paint, whilst cast aluminium requires no pre-treatment other than removal of dirt and grease.

Lead and brass are best left unpainted as paints do not adhere well to these surfaces. Copper must be well abraded before the application of paint.

Preparation:

New:
Clean to remove grease, dirt, oil, etc., by washing with a suitable concentrated detergent.

Previously painted:
If in poor condition, remove with Dekro Paint Stripper. Then proceed as for new work. If in good condition, clean down thoroughly with suitable solvent to remove dirt, grease, oil, etc. Sand glossy surfaces. Dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Glass Specialist surfaces & applications

General:

Glass does not present a very good surface for painting as it is extremely smooth. Nevertheless, extensive painting, mainly in the form of signwriting is carried out on glass using High Gloss Enamel and frosting using Semi-Gloss and Matt Enamels or Plastic Emulsion paints. Whenever possible, glass should be painted on the unexposed side.

Preparation:

New:
Wash down well with a suitable concentrated detergent solution to remove dust, dirt, greasiness from handling, etc. Wipe down glass using methylated spirit and clean cloths.

Previously painted:
Remove existing paint by scraping, or with Dekro Super Paint Stripper. Then proceed as for new work. If in good condition, clean down thoroughly with a suitable solvent to remove dirt, grease, oil, etc. Sand glossy surfaces. Dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Fibreglass Specialist surfaces & applications

General:

Fibreglass consists of a polyester resin reinforced with glass fibre, cured and hardened chemically through the use of catalysts. It is inherently resistant to weather and chemicals and is painted purely for decoration.

Preparation:

New:
Wash down well with a suitable concentrated detergent solution to remove mould release agents. Rinse with clean water. Sandpaper lightly and dust off. Sandpaper paint in good condition and dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Plastic Specialist surfaces & applications

General:

The term “plastic” today covers a very wide range of products of different compositions and characteristics. Because of their great physical strength and corrosion resistance polyethylene and P.V.C. piping are extensively used in the building industry as gutters, downpipes, etc. Many of these are self-coloured, but may require painting on occasion to blend in with the general colour scheme of the structure.

Preparation:

New:
Remove dust, dirt, oil, etc., by washing down with a suitable concentrated detergent solution. Then abrade with a suitable sandpaper to roughen the surface slightly. This is necessary to ensure good adhesion of the paint.

Previously painted:
If in poor condition, remove by scraping, sandpapering, etc. Do not use paint remover. If in good condition clean down and sandpaper lightly. Dust off.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Canvas Specialist surfaces & applications

General:

Special products such as copper and zinc napthenate are used for the preservation on canvas. Oils, bitumens and waxes are used for impregnation and waterproofing. All these materials posses the necessary flexibility to withstand constant folding and unfolding. Paints as a rule do not posses the required flexibility, but on the odd occasion some form of painting may be required, e.g. awnings, sails, canoes, etc.

Preparation:

Remove gross contamination.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Floors Specialist surfaces & applications

General:

When old floors, whether wood, cork, stone, steel, are painted or varnished, special care should be taken that no wax or polish remains on the surface before the paint or varnish coat is applied. Wax polish can be removed from cement floors by scrubbing with a suitable concentrated detergent solution or Dekro Wunda Clean followed by acid etch, but on wood and cork floors only machine sanding will be effective. Floors covered with linoleum or synthetic/rubberised tiles do not normally take surface coatings.

New cement or stone surfaces must be completely dry and fully hydrated before application of paint or varnish.

Preparation:

New:
Clean down to remove dust, dirt or other contamination.

Previously painted or varnished but not polished:
If in poor condition, remove existing coat to original surface by scraping or with Dekro Paint Stripper. Clean down thoroughly and allow to dry. If in good condition, clean down and sandpaper lightly.

Previously wax polished:
Machine sand wood or cork floors. Dust off. Scrub cement floors with a suitable concentrated detergent solution, followed by an acid etch. Wash down with clean water and allow to dry.

N.B.: It is essential to apply a test patch prior to the application of a floor coating to ensure compatibility, intercoat adhesion, wax removal, etc.

N.B.: We recommend that one of our expert technicians be consulted before coating any floor.

CEMENT FLOORS

Twin Packs (Interior/Exterior)

First coat: Dekro Suitable Twin Pack thinned 20% with Suitable thinners
Second coat: Dekro Suitable Twin Pack
Third coat: Dekro Suitable Twin Pack

Single Packs (Interior/Exterior)

First coat: Dekro Suitable Single Pack Thinned 10% with suitable thinners.
Second coat: Dekro Suitable Single Pack

Note: Intended for dry cement surfaces, but can be used on wood and suitably primed steel. A reasonablepriced product for areas with light traffic

Roads And Signs Specialist surfaces & applications

General:

Paint is used extensively for marking road surfaces, kerbs and road signs, as an aid to order and safety.

Preparation:

New:
Bitumen or concrete roads must be dry. Sweep thoroughly to remove dust, loose dirt and gravel.

Previously painted:
Sweep to remove loose paint, dust, dirt and gravel.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat

Bituminous and Creosoted Surfaces Specialist surfaces & applications

General:

Bituminous paints do not lend themselves to overcoating with ordinary decorative paints, as they usually bleed through after a time and stain the finishing coat brown. Bituminous paints have the disadvantage of being very thermoplastic and finishing coats that cannot cope with the expansion and contraction will tend to crack.

Where removal of the coating is not possible, the continued use of a bituminous material is advised. If the bulk of the bitumen has been removed, painting can be carried out reasonably successfully. Creosote or similar wood preservatives cause discolouration (bleeding) and slow drying of ordinary decorative paints.

When aged, they can be painted reasonably successfully over a suitable sealer.

Preparation:
Painting over thick, soft bituminous coatings or over freshly creosoted timber is not advised. If the bitumen coating is thin and hard, and the creosote well aged, clean down to remove all dirt, dust and grease. Scrape off all loose and flaking material to a firm base.

Previously painted:
Sweep to remove loose paint, dust, dirt and gravel.

First Coat: Hydrolock Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Dekro Bituminous Aluminium (Exterior)

First coat: Dekro Bituminous Aluminium
Second coat: Dekro Bituminous Aluminium

Dekro Standard Aluminium Paint (Interior/Exterior)

First coat: Dekro Standard Aluminium Paint
Second coat: Dekro Standard Aluminium Paint

Chemical Resistant Specialist surfaces & applications

General:

Paint systems which are resistant to particular chemicals such as alkalies, acids, solvents, detergents, oils, fats, etc., are frequently required. Where chemically resistant paints are required, two main types are available, namely:

  1. i) Epoxy Enamel, based on epoxy resins
  2. ii) Dekro Adthane Polyurethane Enamel (Urethane Acrylic)

It is essential to read thoroughly the comprehensive data sheets to ascertain the correct coating for the particular type of chemical resistance required. We recommend that one of our expert technicians be consulted before coating any important structure.

In each case careful attention must be given to preparation of surfaces, as thorough cleaning and preparation play a particularly important part in high chemical corrosion resistance. Thickness of the coating is of great importance where conditions are severe. Where these coatings have to be used primers and undercoats of the same type must generally be employed, as orthodox primers and undercoats are not always compatible.

Finally it should be noted that in constantly corrosive conditions individual coats would become contaminated if left for too long before further coats are applied. Successive coats should therefore be applied without delay.

Preparation:

New:
Prepare new surfaces as previously outlined under the appropriate headings.

Previously painted:
If in poor condition, remove all paint back to the original surface, by scraping, wirebrushing, burning, sanding or with Dekro Paint Stripper.

Dekro Epicon Epoxy Enamel may be applied satisfactorily over existing paint, provided it is hard, in good condition, cleaned down and lightly sanded. Some paints, however, may soften or lift and it is recommended to assess this by small-scale trials. If the existing paint is not satisfactory in this respect, it must be stripped to the original surface.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Heat Resistant Specialist surfaces & applications

General:

Fluctuations in temperature impose more strain of the paint film than lengthy exposure to a steady temperature.

The resistance to moisture and chemical attack diminishes after long exposure at high temperatures. It may be found that a film will withstand several months exposure to high temperature, but may fail rapidly if the plant is closed down and moisture allowed to condense on the surface.

Surfaces subjected to heat or steam radiators, steam coil sand pipes, drying ovens, metal flues, chimneys, smoke stacks, etc.

Preparation:

New:
Hose or rinse down with clean water to remove heavy dust, grit or organic matter. Clean down with Dekro Galv-O-Clean Degreaser by working over the surface using a mop, brush or hessian. Thoroughly rinse down with clean water to remove residues. Note whether the final rinsing water forms a continuous film over the surface. If it does, then cleaning is sufficient; if not, repeat the cleaning operation.

Previously painted Section:
If the existing paint is in poor condition, remove by scraping, burning or with Dekro Super Paint Stripper. Then proceed as for new work. If the existing paint is in good condition wash down to remove dirt, grease, dust or other contaminants with a suitable concentrated detergent. Abrade glossy surfaces with a suitable abrasive and dust off.

100ºC – 200ºC

Apply Dekro Heat Resistant Aluminium paint directly to clean bare metal. Raise temperatures to 150ºC and maintain for one hour to precure before reaching normal working temperature.

100ºC – 400ºC

Apply Dekro Silicon NO.400 aluminium directly to clean metal.

Freeze Resistant Specialist surfaces & applications

General:

Temperatures below 5ºC will prevail in most cold storage rooms, the actual operating temperature depending on the particular food product being preserved.

A further requirement would be resistance to various destructive influences such as water and ice, salts, fats, oils, blood, fruit juices, etc. The paint coating used must also be non-toxic and should not taint food.

Two main products are recommended:
Dekro Hydrosilk for plaster surfaces and Clorinated Rubber for all metals, wood, composition board and plaster.

Preparation:

New:
Prepare the various surfaces as described under the appropriate headings.

Previously painted:
Prepare the various surfaces as described under the appropriate headings. Particular care must be taken to remove all traces of contaminants such as fats, oils, salts, etc.

Where Epoxy Enamel is to replace an old non-epoxy coating, the old coating must be removed completely if not compatible.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Fungus and Algae Resistant Specialist surfaces & applications

General:

Fungi (mildew or moss) are a low form of plant life existing in hundreds of species. The growth of a specie depends on the particular conditions which suit it, e.g. continuous high humidity, temperature, lack of light and sunshine, still air or whether the base is a nutrient, etc.

Fungus growth occurs in damp rooms and buildings such as lavatories, basements, laundries, breweries, cellars, etc., and outdoors, particularly on asbestos cement roofs. Fungi may remain dormant for long periods under dry conditions, but are activated when the humidity rises above a certain level.

Algae often occur in south-facing walls during the damp rainy season and are recognised by the bright green colour which appears when completely dry.

Preparation:

New:
Where growth is expected to occur, surfaces should first be washed down with Hydrowash Fungicidal to destroy any spores on the surface.

Previously painted:
Badly infected films must be completely removed to the original surface which must then be treated with Hygiene Solution Primers.

Then proceed as for new work.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Waterproofing Specialist surfaces & applications

Asbestos-containing or suspected materials

Do not scrape, sand, dry-brush or pressure-clean material that may contain asbestos. Stop and seek advice from a suitably qualified asbestos specialist before any preparation or coating work. Read NIOH asbestos guidance.

General:

Dekro Rainproof system can be used on: new concrete roofs (after full curing of concrete), asbestos roofs, galvanised iron roofs, new timber roofs, expansion joints and flashings. Also on roofs previously treated with Asphalt, Malthoid or similar combination roof coverings.

Preparation:

STANDARD APPLICATION PROCEDURE:

  1. Apply to the substrate one primer / sealer coat of Rainproof, diluted with 20% water and allow to dry (drying time is ± 4 hours at standard condition 25ºC and 50% humidity).

  1. Apply one coat of Rainproof as supplied, to an area not exceeding one metre by the width of the Polyester Fabric used (Bidum) and firmly press the fabric into the coating, before the Rainproof coating begins to dry. Repeat the process in one metre lengths at a time. Allow the application to dry before proceeding. (Drying time is ±4 hours at standard condition 25ºC and 50% humidity). If the polyester fabric becomes rain saturated, allow to dry out completely over an extended period before proceeding with the application process.

  1. Apply one coat of Rainproof, diluted with 20% water, to penetrate and saturate the Polyester fabric (Bidum) surface. Allow the application to dry thoroughly before proceeding. (Drying time is ±4 hours at standard condition at 25ºC and 50% humidity).

  1. Finally apply two coats of Rainproof as supplied, allowing to dry between coats. (Drying time per coat is ±4 hours at standard condition 25ºC and 50% humidity).

New Concrete Roofs:
Screeding to be inspected and made good if necessary. Scrape all loose materials and sweep clean. Apply standard application procedures 1 – 4.

Roofs previously treated with old Asphalt, Malthoid or similar combinations:
Remove all loose material, clean out and fill cracks. Wash and brush down roof to clean surface. Apply standard application procedures 1 – 4.

Galvanised Iron Roofs:
Wire brush and wash down to remove all surface contamination. Treat rust areas with rust neutraliser after sandpapering. Treat screw heads by priming with Hydrobond 44. Treat minor holes by applying one coat Rainproof as supplied. Press into the coating a suitable patch of Polyester Fabric (Bidum) before the coating dries.

Apply one coat of Rainproof, diluted with 20% water, over the patched-up area. Allow to dry. Apply to the entire area, including patches, two coats of Rainproof as supplied, allowing to dry between coats.

New Timber Roofs:
Ensure that the timber is completely dry. Apply standard application procedures 1 – 4.

Flashings:
Apply standard application procedures 1 – 4, ensuring that the ends of the Polyester Fabric (Bidum) are not exposed.

First Coat: Suitable Dekro Primer
Second Coat: Suitable Top Coat
Third Coat: Suitable Top Coat

Guide filtered.